The plasma etching methods for minimizing mask CD variation by cleaning process
Format Member Price Non-Member Price
PDF $14.40 $18.00
cover GOOD NEWS! Your organization subscribes to the SPIE Digital Library. You may be able to download this paper for free. Check Access

Paper Abstract

There has been a growing demand for more precise Mask CD MTT (Critical Dimension Mean to Target) control by shrinking the semiconductor device. Generally, The CD MTT is determined by patterning process such as writing, develop, and etch. But, additional CD MTT variation often occurs by cleaning process after patterning process. As a result, it is important to preserve the CD MTT for minimizing CD variation by cleaning process. The cleaning process of photomask is becoming more critical for 32nm node and below because the size of defect and SRAF pattern is in the same range. In order to achieve high first cleaning pass yields, intensive cleaning method depending on media not physical force is still essential to photomask manufacturing and these cleaning processes bring about considerable CD MTT change. Therefore, it is necessary to increase the durability of MoSi material of attenuated HTPSM (Half Tone Phase Shift Mask) by the new surface treatment method. In this study, we presented the plasma etching technique for Cr strip etch in the 2nd process of the attenuated HTPSM for minimizing CD variation by cleaning process. Diverse dry etching processes are investigated to improve the durability of the MoSi patterns. In order to evaluate the surface modification of the MoSi film, surface compositions are analyzed by XPS (X-ray Photoelectron Spectroscopy), TOF-SIMS (Time of Flight Secondary Ion Mass Spectrometry), and EELS (Electron Energy Loss Spectroscopy). The variation of CD MTT and optical properties are also evaluated by CD SEM and AIMS (Aerial Image Measurement System), respectively. The XPS analysis shows that sidewall passivation films are formed during the main etch process and then modified at the over etch step and additional in-situ O2 plasma treatment. The concentration of the MoO3 is increased when over etch step and in-situ O2 plasma treatment are added. The difference of CD shift between initial measurement and 2nd measurement after cleaning process depends on plasma etching conditions. Consequently, the increase in the peak intensity of MoO3 that is less soluble than that of MoO2 leads to preserve CD by cleaning chemicals.

Paper Details

Date Published: 8 November 2012
PDF: 7 pages
Proc. SPIE 8522, Photomask Technology 2012, 852215 (8 November 2012); doi: 10.1117/12.964984
Show Author Affiliations
Hyun Duck Shin, SKHynix Inc. (Korea, Republic of)
Soo Kyeong Jeong, SKHynix Inc. (Korea, Republic of)
Ho Yong Jung, SKHynix Inc. (Korea, Republic of)
Sang Pyo Kim, SKHynix Inc. (Korea, Republic of)
Dong Gyu Yim, SKHynix Inc. (Korea, Republic of)


Published in SPIE Proceedings Vol. 8522:
Photomask Technology 2012
Frank E. Abboud; Thomas B. Faure, Editor(s)

© SPIE. Terms of Use
Back to Top