Paper Abstract

BRDF at 3.39 microns was measured on silicon carbide and aluminum foam and on 401C10 black paint. BRDF of the black paint increases by a factor of 100 at glancing angle. BRDF of the foams increases by less than a factor of 10 at glancing angle.