Fast and accurate scatterometry metrology method for STI CMP step height process evaluation
Author(s): Chih-Hsun Lin; Climbing Huang; Chia-Lin Hsu; Wu-Sian Sie; J. Y. Wu; Ching-Hung Bert Lin; Zhi-Qing James Xu; Qiong-Yan Yuan; Sungchul Yoo; Chien-Jen Eros Huang; Chao-Yu Harvey Cheng; Juli Cheng; Zhiming Jiang; Houssam Chouaib
Format Member Price Non-Member Price
PDF $14.40 $18.00
cover GOOD NEWS! Your organization subscribes to the SPIE Digital Library. You may be able to download this paper for free. Check Access

Paper Abstract

At the 28nm node using 300mm wafers, oxide step height in STI CMP transient gate after-etch inspection (TG AEI) wafers is a critical parameter that affects device performance and should be monitored and controlled. For production process control of this kind of structure, a metrology tool must utilize a non-destructive measurement technique, and have high sensitivity, precision and throughput [1]. This paper discusses a scatterometry-based measurement method for monitoring critical dimension step height in STI CMP instead of traditional measurement methods such as atomic force microscopy (AFM). The scatterometry tool we used for our investigations was the KLA-Tencor SpectraShape 8810, which is the most recent model of the spectroscopic critical dimension (SCD) metrology tools that have been implemented in production for process control of TG AEI structures. AFM was used as a reference metrology technique to assess the accuracy performance of the SpectraShape8810. The first objective of this paper is to discuss the best azimuth angle and floating parameters for scatterometry measurement of the step height feature in TG AEI wafers. Second, this paper describes the tool matching performance of SpectraShape 8810 and correlation to AFM determined using a DOE of TG AEI wafers.

Paper Details

Date Published: 5 April 2012
PDF: 8 pages
Proc. SPIE 8324, Metrology, Inspection, and Process Control for Microlithography XXVI, 832421 (5 April 2012); doi: 10.1117/12.916235
Show Author Affiliations
Chih-Hsun Lin, United Microelectronics Corp. (Taiwan)
Climbing Huang, United Microelectronics Corp. (Taiwan)
Chia-Lin Hsu, United Microelectronics Corp. (Taiwan)
Wu-Sian Sie, United Microelectronics Corp. (Taiwan)
J. Y. Wu, United Microelectronics Corp. (Taiwan)
Ching-Hung Bert Lin, KLA-Tencor Corp. (United States)
Zhi-Qing James Xu, KLA-Tencor Corp. (United States)
Qiong-Yan Yuan, KLA-Tencor Corp. (United States)
Sungchul Yoo, KLA-Tencor Corp. (United States)
Chien-Jen Eros Huang, KLA-Tencor Corp. (United States)
Chao-Yu Harvey Cheng, KLA-Tencor Corp. (United States)
Juli Cheng, KLA-Tencor Corp. (United States)
Zhiming Jiang, KLA-Tencor Corp. (United States)
Houssam Chouaib, KLA-Tencor Corp. (United States)


Published in SPIE Proceedings Vol. 8324:
Metrology, Inspection, and Process Control for Microlithography XXVI
Alexander Starikov, Editor(s)

© SPIE. Terms of Use
Back to Top