Fabrication and characteristic of long photonic crystal fiber taper
Author(s): Peiguang Yan; Huifeng Wei; Shuangchen Ruan; Su Chen; Chunyu Guo; Jiangtao Guo; Jie Shu; Guangzhong Cao
Format Member Price Non-Member Price
PDF $14.40 $18.00

Paper Abstract

In this paper, we drew a 500 m-long PCF taper directly on the industry drawing tower. The fiber taper has a uniform cross-section structure with OD from 170 μm to 70 μm, and demonstrates very good beam quality. The optical attenuation of PCF taper was measured. The optical attenuation is ~5 dB/km near 1200 nm, but the water absorption peak around 1400 nm and the attenuation beyond 1600 nm are still large. The zero dispersion wavelength (ZDW) was calculated to be ~1090 nm at the taper input end, and shifted to ~870 nm at the taper output end. The PCF taper was pumped with a picosecond laser source at wavelength of 1064 nm, and generated 200 mW output power of SC covering from ~450 nm to 1600 nm.

Paper Details

Date Published: 15 February 2012
PDF: 6 pages
Proc. SPIE 8240, Nonlinear Frequency Generation and Conversion: Materials, Devices, and Applications XI, 82401R (15 February 2012); doi: 10.1117/12.909796
Show Author Affiliations
Peiguang Yan, Shenzhen Univ. (China)
Huifeng Wei, Yangtze Optical Fibre and Cable Co., Ltd. (China)
Shuangchen Ruan, Shenzhen Univ. (China)
Su Chen, Yangtze Optical Fibre and Cable Co., Ltd. (China)
Chunyu Guo, Shenzhen Univ. (China)
Jiangtao Guo, Yangtze Optical Fibre and Cable Co., Ltd. (China)
Jie Shu, Shenzhen Univ. (China)
Guangzhong Cao, Shenzhen Univ. (China)


Published in SPIE Proceedings Vol. 8240:
Nonlinear Frequency Generation and Conversion: Materials, Devices, and Applications XI
Konstantin L. Vodopyanov, Editor(s)

© SPIE. Terms of Use
Back to Top