Laser cladding of protective coatings of limited cracking susceptibility
Author(s): Rafal Jendrzejewski; Gerard Sliwinski; Marek Krawczuk; Wieslaw M. Ostachowicz
Format Member Price Non-Member Price
PDF $14.40 $18.00
cover GOOD NEWS! Your organization subscribes to the SPIE Digital Library. You may be able to download this paper for free. Check Access

Paper Abstract

During direct laser cladding process teh substrate preheating temperature is selected together with interaction parameters of the 1.2 kW cw CO2 laser source. The Co-based protective coatings are prepared on chromium steel. A decrease of cracking susceptibility with increasing substrate temperature follows from the model calculation of the temperature and stress fields and is confirmed in experiment. For laser intensities around 108 W/m2 and preheating above 600°C the crack-free 2-layer coatings are produced.

Paper Details

Date Published: 23 March 2005
PDF: 4 pages
Proc. SPIE 5777, XV International Symposium on Gas Flow, Chemical Lasers, and High-Power Lasers, (23 March 2005); doi: 10.1117/12.611284
Show Author Affiliations
Rafal Jendrzejewski, Szewalski Institute of Fluid-Flow Machinery (Poland)
Gerard Sliwinski, Szewalski Institute of Fluid-Flow Machinery (Poland)
Marek Krawczuk, Szewalski Institute of Fluid-Flow Machinery (Poland)
Wieslaw M. Ostachowicz, Szewalski Institute of Fluid-Flow Machinery (Poland)


Published in SPIE Proceedings Vol. 5777:
XV International Symposium on Gas Flow, Chemical Lasers, and High-Power Lasers
Jarmila Kodymova, Editor(s)

© SPIE. Terms of Use
Back to Top