To characterize the S-N curve form in gigacycle fatigue, five high strength low alloy steels with tensile strengths from 1500 MPa to 1800MPa were tested at very high numbers of cycles through piezoelectric fatigue test at 20 KHz. A significant change in the slope of S-N curve was observed, accompanying the transition form surface to subsurface crack initiation. The S-N diagram on these steels reveals a two-stepwise shape, and the S-N curve tends to drop down again after 107 or 108 cycles. The specimens continue to fail over 107 stress cycles. It should be significant to realize the risk of obtaining the fatigue limit at 107 cycles.

Paper Details

Date Published: 29 May 2002
PDF: 4 pages
Proc. SPIE 4537, Third International Conference on Experimental Mechanics, (29 May 2002); doi: 10.1117/12.468825
Show Author Affiliations
Q. Y. Wang, Sichuan Univ. (China)
C. Bathias, ITMA-CNAM (France)
N. Kawagoishi, Kagoshima Univ. (Japan)
Q. Chen, Kagoshima Univ. (Japan)


Published in SPIE Proceedings Vol. 4537:
Third International Conference on Experimental Mechanics

© SPIE. Terms of Use
Back to Top